• English
    • Ελληνικά
    • Deutsch
    • français
    • italiano
    • español
  • Deutsch 
    • English
    • Ελληνικά
    • Deutsch
    • français
    • italiano
    • español
  • Einloggen
Dokumentanzeige 
  •   DSpace Startseite
  • Επιστημονικές Δημοσιεύσεις Μελών ΠΘ (ΕΔΠΘ)
  • Δημοσιεύσεις σε περιοδικά, συνέδρια, κεφάλαια βιβλίων κλπ.
  • Dokumentanzeige
  •   DSpace Startseite
  • Επιστημονικές Δημοσιεύσεις Μελών ΠΘ (ΕΔΠΘ)
  • Δημοσιεύσεις σε περιοδικά, συνέδρια, κεφάλαια βιβλίων κλπ.
  • Dokumentanzeige
JavaScript is disabled for your browser. Some features of this site may not work without it.
Gesamter Bestand
  • Bereiche & Sammlungen
  • Erscheinungsdatum
  • Autoren
  • Titeln
  • Schlagworten

Tensile and fatigue behaviour of wrought magnesium alloys AZ31 and AZ61

Thumbnail
Autor
Chamos, A. N.; Pantelakis, S. G.; Haidemenopoulos, G. N.; Kamoutsi, E.
Datum
2008
DOI
10.1111/j.1460-2695.2008.01267.x
Schlagwort
fatigue
fracture mode
tension
texture
twinning
MECHANICAL-PROPERTIES
NONBASAL SLIP
MICROSTRUCTURE
DEFORMATION
ANISOTROPY
Engineering, Mechanical
Materials Science, Multidisciplinary
Zur Langanzeige
Zusammenfassung
The mechanical behaviour of two hot rolled magnesium alloys, namely the AZ31 and AZ61, has been evaluated experimentally under both monotonic and cyclic loading. Both longitudinal (L) and long transverse (LT) directions were evaluated. The tensile behaviour of the L and LT directions is similar and differs only in the offset 0.2% yield strength for both materials. This difference is attributed to the angular spread of basal poles toward the rolling direction and is more pronounced for the case of AZ31. A distinct hardening response is obvious in both directions. Twinning formation was observed; it is more pronounced in the longitudinal direction while the fracture mode is intergranular and equiaxed facets are present in the fracture surfaces of the specimens. The S-N curves exhibit a smooth transition from the low to high cycle fatigue regime. AZ61 exhibits an overall better fatigue behaviour compared to AZ31. A transgranular crack initiation mode is observed in all tested specimens while the propagation of the cracks is characterized as intergranular.
URI
http://hdl.handle.net/11615/26554
Collections
  • Δημοσιεύσεις σε περιοδικά, συνέδρια, κεφάλαια βιβλίων κλπ. [19735]
htmlmap 

 

Stöbern

Gesamter BestandBereiche & SammlungenErscheinungsdatumAutorenTitelnSchlagwortenDiese SammlungErscheinungsdatumAutorenTitelnSchlagworten

Mein Benutzerkonto

EinloggenRegistrieren
Help Contact
DepositionAboutHelpKontakt
Choose LanguageGesamter Bestand
EnglishΕλληνικά
htmlmap