Mostra i principali dati dell'item
Preparation of graphitic mesoporous carbon for the simultaneous detection of hydroquinone and catechol
dc.creator | Yuan, X. | en |
dc.creator | Yuan, D. | en |
dc.creator | Zeng, F. | en |
dc.creator | Zou, W. | en |
dc.creator | Tzorbatzoglou, F. | en |
dc.creator | Tsiakaras, P. | en |
dc.creator | Wang, Y. | en |
dc.date.accessioned | 2015-11-23T10:54:27Z | |
dc.date.available | 2015-11-23T10:54:27Z | |
dc.date.issued | 2013 | |
dc.identifier | 10.1016/j.apcatb.2012.09.017 | |
dc.identifier.issn | 9263373 | |
dc.identifier.uri | http://hdl.handle.net/11615/34745 | |
dc.description.abstract | A graphitic mesoporous carbon (GMC) had been successfully synthesized using Ni-Fe layered double hydroxide (LDH) as both template and catalyst under a relatively low pyrolysis temperature. The techniques of X-ray diffraction, transmission electron microscopy, Raman spectrum and N2 adsorption/desorption were used to characterize the physico-chemical properties of the as-prepared GMC. Meanwhile, the voltammetric behaviors of hydroquinone (HQ) and catechol (CC) were studied at the GMC modified glassy carbon electrode (GMC/GCE). The separation of the oxidation and reduction peak (ΔEp) for HQ and CC were decreased from 369 to 42mV and from 365 to 52mV, respectively, and the anodic peak currents for the oxidation of both HQ and CC were also remarkably increased at the GMC/GCE. Furthermore, at the GMC/GCE, the two components could be entirely separated with a large oxidation peak potential separation between HQ and CC. Under the optimized condition, the peak currents of HQ and CC increased linearly with increasing HQ and CC contents. The detection limit for HQ and CC was 3.7×10-7 and 3.1×10-7molL-1, respectively. © 2012 Elsevier B.V. | en |
dc.source | Applied Catalysis B: Environmental | en |
dc.source.uri | http://www.scopus.com/inward/record.url?eid=2-s2.0-84868559553&partnerID=40&md5=c26a6c0878b47d6170a28303dcfdccf7 | |
dc.subject | Graphitic mesoporous carbon | en |
dc.subject | Layered double hydroxides | en |
dc.subject | Simultaneous detection of hydroquinone and catechol | en |
dc.subject | Adsorption/desorption | en |
dc.subject | Anodic peaks | en |
dc.subject | Detection limits | en |
dc.subject | Mesoporous carbon | en |
dc.subject | Modified glassy carbon electrode | en |
dc.subject | Optimized conditions | en |
dc.subject | Oxidation and reduction | en |
dc.subject | Oxidation peak | en |
dc.subject | Peak currents | en |
dc.subject | Physicochemical property | en |
dc.subject | Pyrolysis temperature | en |
dc.subject | Simultaneous detection | en |
dc.subject | Two-component | en |
dc.subject | Voltammetric behaviors | en |
dc.subject | Anodic oxidation | en |
dc.subject | Carbon | en |
dc.subject | Chemical properties | en |
dc.subject | Glass membrane electrodes | en |
dc.subject | Mesoporous materials | en |
dc.subject | Separation | en |
dc.subject | Transmission electron microscopy | en |
dc.subject | X ray diffraction | en |
dc.subject | Phenols | en |
dc.title | Preparation of graphitic mesoporous carbon for the simultaneous detection of hydroquinone and catechol | en |
dc.type | journalArticle | en |
Files in questo item
Files | Dimensione | Formato | Mostra |
---|---|---|---|
Nessun files in questo item. |