Corrosion-induced hydrogen embrittlement in aluminum alloy 2024
(2006)The present paper focuses on the observed corrosion-induced embrittlement of alloy 2024 and tries to answer the key question on whether the observed embrittlement is attributed to hydrogen uptake and trapping in the material. ...